Sign In | Join Free | My himfr.com
Home > Base Metal Casting Alloys >

Density 8.5cm³ Nickel Based Superalloys , Nickel Chromium Alloy Long Cooling Time

    Buy cheap Density 8.5cm³ Nickel Based Superalloys , Nickel Chromium Alloy Long Cooling Time from wholesalers
     
    Buy cheap Density 8.5cm³ Nickel Based Superalloys , Nickel Chromium Alloy Long Cooling Time from wholesalers
    • Buy cheap Density 8.5cm³ Nickel Based Superalloys , Nickel Chromium Alloy Long Cooling Time from wholesalers
    • Buy cheap Density 8.5cm³ Nickel Based Superalloys , Nickel Chromium Alloy Long Cooling Time from wholesalers

    Density 8.5cm³ Nickel Based Superalloys , Nickel Chromium Alloy Long Cooling Time

    Ask Lasest Price
    Brand Name : Willett
    Model Number : NCP25K
    Certification : CE
    Price : Contact for pricing
    Payment Terms : L/C, T/T, Western Union, MoneyGram
    Supply Ability : 50 + KG + per day
    Delivery Time : 5-8 Business days
    • Product Details
    • Company Profile

    Density 8.5cm³ Nickel Based Superalloys , Nickel Chromium Alloy Long Cooling Time

    Nickel Chrome Dental Casting Alloys for Porcelain and Ceramic


    Our Nickel Chrome dental alloy is a Nickel-based alloy that possess an excellent workability and absolutely versatile characteristics. It compates with most ceramics powders seamlessly. Thanks to Willett's patented special formula, it consisted superior bonding strength compares to other competitors.


    This packaging of 25KG is specially made for Wholesale purpose.


    Please let our sales representative know your packaging preference. We are also able to provide retail packaging alongside with the shipment.


    *Customers can choose with NCP engraved or without.


    Elements

    NiCrOthersCTEVHNElongation
    60.5-62.5%25.2-27.3%10.2-14.3%14-14.1270HV104%

    Melting range ℃Density g/ccYield Strength(Rp0.2)
    1260-13508.5cm³500MPa

    Features:


    1. Extremely high resistance to corrosion: no cytotoxic potential in cell culture test

    2. Biocompatibility certified by Both government and third-party institutes

    3. Low thermal conductivity

    4. High modulus of elasticity

    5. Great strength with any acceptable span

    6. Long cooling time not required: low coefficient of expansion

    7. Reliable metal-to-ceramic bond

    8. High heat resistance: consistence of dimensional stability during high-temp pocessing


    FAQ:


    What is the perfect temperature to obtain the best result when casting?


    The casting temperature should always maintain 100~150℃ higher than liquidus temperature.


    What is the perfect timing to obtain the best result when casting?


    While casting Nickel Chrome alloys that don't contain Beryllium, the surface of the melting alloys will appear a layer of shadow. Once the shadow disappears and the edges of the alloy have become rounded (melted until it becomes a sphere shape is not necessary) will be the best timing for casting. Perfect timing for casting Cobalt Chrome alloy is to heat it till the surface membrane perforated and a spark of bright light start to appear.


    Cobalt Chrome casting piece is incomplete, what are the causes?


    1. Casting ring is not heated evenly: While casting Cobalt alloys, casting ring must heat up gradually and slowly before reaches 300℃. Let it sit in the oven in between 300℃ and 600℃ for 10-30 minutes. Once it heats up to the desired temperature, maintain the same temperature for at least 30 minutes before casting.


    2. Casting temperature is below/above alloy's requirement.


    3. Strub designed improperly: For example, Strub is too narrow. We strongly recommend the Strub diameter consist of 5mm or more.


    4. The amount of alloy is not enough for the casting piece or the centrifugal force of casting pressure is not enough.


    5. Casting piece has not avoided the heat center.



    Quality Density 8.5cm³ Nickel Based Superalloys , Nickel Chromium Alloy Long Cooling Time for sale
    Inquiry Cart 0